Title: EVALUATION AND PREDICTION OF PITTING RESISTANCE OF HEAT EXCHANGERS MADE OF ALLOY 06KhN28MDT (SIMILAR TO AISI 904L STEEL) IN MODEL CIRCULATING WATERS

EVALUATION AND PREDICTION OF PITTING RESISTANCE OF HEAT EXCHANGERS MADE OF ALLOY 06KhN28MDT (SIMILAR TO AISI 904L STEEL) IN MODEL CIRCULATING WATERS
Anna Dzhus; Sergey Subbotin; Tetiana Pulina; Serhii Leoshchenko; Gennadii Snizhnoi
10.5593/sgem2023/6.1
1314-2704
English
23
6.1
•    Prof. DSc. Oleksandr Trofymchuk, UKRAINE 
•    Prof. Dr. hab. oec. Baiba Rivza, LATVIA
A mathematical model was developed, which is based on a multivariate regression dependence and establishes the relationship between the critical pitting temperature (CPT) of the 06KhN28MDT alloy (similar to AISI 904L steel) and its chemical composition and structural components in model circulating waters with pH 4...8 and chloride concentration from 350 up to 600 mg/liter, which correspond to industrial circulating water during the operation of heat exchangers. Based on the results of the analysis of the developed mathematical model, chemical composition, structural heterogeneity of the studied alloy melts and parameters of model recycled water (pH and chloride concentration), it has been found that the significant variables of the model are the parameters of the media, the mean grain diameter of the austenite of the 06KhN28MDT alloy, and the chromium content in it within the standard for its production. It is shown that the CPT of the 06KhN28MDT alloy increases by 8.3 °C (degree Celsius) with a decrease in the chloride concentration in model recycled water from 600 up to 350 mg/L, by 6.8 °C (degree Celsius) with an increase in its pH from 4 up to 8, by 5.9 °C (degree Celsius) with a decrease in the mean diameter of the austenite grain from 31 to 11 ?m, and by 4.7 °C with a decrease in its chromium content from 24.31 up to 21.84 wt %. It has been found that, under the same research conditions, the parameters of model recycled water have the most significant effect on the CPT of 06KhN28MDT alloy and stainless steels 08Kh18N10, AISI 304, 12Kh18N10T and AISI 321. However, the chromium content and mean austenite grain diameter of the alloy have an opposite effect on its CPT to these steels. This is most likely due to the fact that at such a high chromium concentration and the presence of molybdenum, metastable pittings that occur on its surface are quickly repassivated. This can contribute to the transformation of the remaining pitting into stable pitting at a lower CPT due to the redistribution of the current density between them. The paper substantiates the use of the developed mathematical model to evaluate and predict the pitting resistance of heat exchangers made of 06KhN28MDT alloy under possible changes in the parameters of recycled water (pH and chloride concentration) during their operation, depending on the chromium content and the size of the mean diameter of the austenite grain.
[1] Oh Y.-K., Hwang K.-R., Kim C., et. al. Recent developments and key barriers to advanced biofuels: A short review. Bioresource Technology, 2018, 257, pp. 320-333.
[2] Torres C.E.A.S., Santos T.E., Lins V.F.C. Corrosion failures of austenitic and duplex stainless steels in a biodiesel plant. Revista Materia, 2020, 25 (2), 25 p.
[3] Narivs’kyi O.E. Corrosion fracture of platelike heat exchangers. Materials Science, 2005, 41(1), pp. 122–128. https://doi.org/10.1007/s11003-005-0140-8
[4] Narivs’kyі O. E. Infuence of heterogenety of AISI321 steel on its pitting in chloridecontaining media. Materials Science, 2007, 43(2), pp. 256–264. DOI: https://doi.org/10.1007/s11003-007-0029-9
[5] Mishchenko V. G., Snizhnoi G. V., Narivs'kyy O. Eh. Magnetometric investigations of corrosion behaviour of AISI 304 steel in chloride-containing environment. Metallofizika i noveishie tekhnologii, 2011, 33(6), pp. 769–774.
[6] Narivs’kyi O.E. Micromechanism of corrosion fracture of the plates of heat exchangers. Materials Science, 2007, 43(1), pp. 124–132. https://doi.org/10.1007/s11003-007-0014-3
[7] Wang W., Jenkins P.E., Ren Z. Heterogeneous corrosion behavior of carbon steel in water contaminated biodiesel. Corrosion Science, 2011, 53, pp. 845-849.
[8] Narivskiy A., Atchibayev R., Muradov A., Mukashev K., Yar-Mukhamedov Y. Investigation of electrochemical properties in chloride-containing commercial waters. International Multidisciplinary Scientific GeoConference Surveying Geology and Mining Ecology Management, SGEM, 2018, 18(6.1), pp. 267–274. DOI: 10.5593/sgem2018/6.1/S24.036
[9] Narivskiy А., Yar-Mukhamedova G., Temirgaliyeva. E., Mukhtarova M., Yar- Mukhamedov Y. Corrosion losses of alloy 06 KhN28MDT in chloride-containing commercial waters. International Multidisciplinary Scientific GeoConference Surveying Geology and Mining Ecology Management: SGEM, 2016, 1, pp. 63–70.
[10] Narivs’kyi O. E., Belykov S. B. Pitting resistance of 06KhN28MDT alloy in chloride-containing media. Materials Science, 2008, 44(4), pp. 573–580. https://doi.org/10.1007/s11003-009-9107-5
[11] Freedman D.A. Statistical models: theory and practice. Cambridge University Press, 2005, 458p.
[12] Narivskyi O.E., Belikov S.B., Subbotin S.A., Pulina T.V. Influence of chloridecontaining media on the pitting resistance of AISI 321 steel. Materials Science, 2021, 57(2), pp. 291-297. DOI: https://doi.org/10.1007/s11003-021-00544-z
[13] Narivskyi О.Е., Subbotin S.A., Pulina T.V., Khoma M.S. Assessment and prediction of the pitting resistance of plate-like heat exchangers made of AISI304 steel and operating in circulating waters. Materials Science, 2022, 58, pp. 41–46. DOI: https://doi.org/10.1007/s11003-022-00628-4
[14] Narivs’kyi O., Atchibayev R., Kemelzhanova A., Yar-Mukhamedova G., Snizhnoi G., Subbotin S., Beisebayeva A. Mathematical modeling of the corrosion behavior of austenitic steels in chloride-containing media during the operation of plate-like heat exchangers. Eurasian Chemico-Technological Journal, 2022, 24(4), pp. 295-301. DOI: https://doi.org/10.18321/ectj1473
[15] Park J.O., Matsch S., Bohni H. Effects of temperature and Chloride Concentration on Pit Initiation and Early Pit Growth of Stainless Steel. Journal of The Electrochemical Society, 2002, 149(2), pp. 34-39.
[16] Narivs’kyi О.Е. Corrosion fracture of plate-type heat exchangers. Fiz.-Khim. Mekh. Mater., 2005, 41, №1, pp. 104-108.
[17] Szklarska-Smialowska, Z. Pitting corrosion of metals. National Association of corrosion Engineers. Houston,1986, pp.147-170.
[18] Yar-Mukhamedova G.S., Darisheva A.M., Yar-Mukhamedov E.S. Adsorption of the Components of a Chrome-Plating Electrolyte on Dispersed Corundum Particles. Materials Science, 2019, 54(6), pp. 907–912.
[19] Karakurkchi H.V., Sakhnenko N.D., Korohodska A.N.,.Stepanova I.I., Zyubanova S.I. Features of Plasma-Electrolyte Synthesis of Heterooxide Nanocomposites on Multicomponent Alloys of Valve Metals. Springer Proceedings in Physics, 2023, 280, pp. 123–147.
conference
Proceedings of 23rd International Multidisciplinary Scientific GeoConference SGEM 2023
23rd International Multidisciplinary Scientific GeoConference SGEM 2023, 03 - 09 July, 2023
Proceedings Paper
STEF92 Technology
International Multidisciplinary Scientific GeoConference SGEM
SWS Scholarly Society; Acad Sci Czech Republ; Latvian Acad Sci; Polish Acad Sci; Serbian Acad Sci and Arts; Natl Acad Sci Ukraine; Natl Acad Sci Armenia; Sci Council Japan; European Acad Sci, Arts and Letters; Acad Fine Arts Zagreb Croatia; Croatian Acad Sci and Arts; Acad Sci Moldova; Montenegrin Acad Sci and Arts; Georgian Acad Sci; Acad Fine Arts and Design Bratislava; Turkish Acad Sci.
25-34
03 - 09 July, 2023
website
9215
chloride-containing media, pitting, critical pitting temperature (CPT), mathematical model, evaluation and prediction of pitting resistance AISI 904L stainless steel