ANALYSIS OF MICROMECHANICAL PROPERTIES OF REACTIVE EXTRUSION COMPOSITES BY NANOINDENTATION

Margarita Natova, Maria Datcheva, . Roumen Iankov, Vassil Georgiev

First published: 2013-06-20https://doi.org/10.5593/sgem2013/bf6/s24.002View metrics

Publication Impact Profile

Publication details

Title
ANALYSIS OF MICROMECHANICAL PROPERTIES OF REACTIVE EXTRUSION COMPOSITES BY NANOINDENTATION
Authors
Margarita Natova, Maria Datcheva, . Roumen Iankov, Vassil Georgiev
Proceedings
SGEM International Multidisciplinary Scientific GeoConference EXPO Proceedings; 13th SGEM GeoConference NANO, BIO AND GREEN TECHNOLOGIES FOR A SUSTAINABLE FUTURE
Publisher
Stef92 Technology
Year
2013
Pages
11 - 16 pp
ISSN
1314-2704
ISBN
Not available yet
Language
en
Publication type
Conference Paper
Keywords
References16
  1. Cartier H. & Guo-Hua Hu A novel reactive extrusion process for compatibilizing immiscible polymer blends, Polymer, vol. 42/issue 21, pp. 8807-8816, 2001.

  2. Natova M., Georgiev V. & Dikov V. A review of current methods for processing of filled polymer composites – developments and future prospects, 11th International Interdisciplinary Scientific Geoconference SGEM 201 1, 20 -26 June 201 1, Albena, Bulgaria, Proceedings Vol. II, pp. 679-686.

  3. Oliver W. & Pharr G. Measurement of Hardness and Elastic Modulus by Instrumented Indentation: Advances in Understanding and Refinement, J. of Mat. Research, vol. 19/issue 1, pp. 3-20, 2004.

  4. Datcheva M., Cherneva S., Stoycheva M., Iankov R. & Stoychev D. Determination of Anodized Aluminum Material Characteristics by Means of Nano-Indentation Measurements, Materials Sciences and Applications, v ol. 2/issue 10, pp. 1452 -1464, 2011.

  5. Bencomo-Cisneros J. A., Tejeda-Ochoa A., García-Estrada J. A., Herre ra-Ramírez C. A., Hurtado-Macías A., Martínez-Sánchez R., & Herrera-Ramírez J. M. Characterization of Kevlar-29 fibers by tensile tests and nanoindentation, Journal of Alloys and Compound, vol. 536S/Supplement 1, pp. S456– S459, 2012.

  6. Riekel C., Dieing T., Engström P., Vincze L., Martin C. & Mahendrasingam A. X- ray Microdiffraction Study of Chain Orientation in Poly(p-phenylene terephthalamide) , Macromolecules vol. 32/issue 23, pp. 7859–7865, 1999.

  7. Roth S., Burghammer M., Janotta A. & Riekel C. Rotational Disorder in Poly(p- phenylene terephthalamide) Fibers by X-ray Diffraction with a 100 nm Beam, Macromolecules, vol. 36/issue 5 1585–1593, pp 1585–1593, 2003.

  8. Davies R. J., Burghammer M. & Riekel C. Simultaneous Microfocus Raman and Microfocus XRD: Probing the Deformation of a Single High -Performance Fiber , Macromolecules, vol. 39/issue 14, pp 4834–4840, 2006.

  9. Cartier H. & Guo-Hua Hu A novel reactive extrusion process for compatibilizing immiscible polymer blends, Polymer, vol. 42/issue 21, pp. 8807-8816, 2001.

  10. Natova M., Georgiev V. & Dikov V. A review of current methods for processing of filled polymer composites – developments and future prospects, 11th International Interdisciplinary Scientific Geoconference SGEM 201 1, 20 -26 June 201 1, Albena, Bulgaria, Proceedings Vol. II, pp. 679-686.

  11. Oliver W. & Pharr G. Measurement of Hardness and Elastic Modulus by Instrumented Indentation: Advances in Understanding and Refinement, J. of Mat. Research, vol. 19/issue 1, pp. 3-20, 2004.

  12. Datcheva M., Cherneva S., Stoycheva M., Iankov R. & Stoychev D. Determination of Anodized Aluminum Material Characteristics by Means of Nano-Indentation Measurements, Materials Sciences and Applications, v ol. 2/issue 10, pp. 1452 -1464, 2011.

  13. Bencomo-Cisneros J. A., Tejeda-Ochoa A., García-Estrada J. A., Herre ra-Ramírez C. A., Hurtado-Macías A., Martínez-Sánchez R., & Herrera-Ramírez J. M. Characterization of Kevlar-29 fibers by tensile tests and nanoindentation, Journal of Alloys and Compound, vol. 536S/Supplement 1, pp. S456– S459, 2012.

  14. Riekel C., Dieing T., Engström P., Vincze L., Martin C. & Mahendrasingam A. X- ray Microdiffraction Study of Chain Orientation in Poly(p-phenylene terephthalamide) , Macromolecules vol. 32/issue 23, pp. 7859–7865, 1999.

  15. Roth S., Burghammer M., Janotta A. & Riekel C. Rotational Disorder in Poly(p- phenylene terephthalamide) Fibers by X-ray Diffraction with a 100 nm Beam, Macromolecules, vol. 36/issue 5 1585–1593, pp 1585–1593, 2003.

  16. Davies R. J., Burghammer M. & Riekel C. Simultaneous Microfocus Raman and Microfocus XRD: Probing the Deformation of a Single High -Performance Fiber , Macromolecules, vol. 39/issue 14, pp 4834–4840, 2006.

View or Download full articleAccess options
Full paper accessChoose SWS login, librarian support, or instant article download.

SWS access login

Login as SWS Scientific Committee

Authors and approved SWS contributors will read and export their own linked papers after identity matching by SWS profile, email and SGEM GlobalID.

For librarian assistance: [email protected]

Purchase Instant Access

48-hour online accessComing soon
Online-only accessComing soon
Download the full article in PDF formatEUR 35
  • Article can be downloaded after successful payment.
  • Article may be used according to SWS library access terms.
  • Article cannot be redistributed.
Get full paper

Back to publication list

Connected events

SGEM WORLD SCIENCE Conferences

The EPS Library connects published research with the scientific events where it was presented, reviewed and prepared for long-term scholarly discovery.

International Scientific GeoConference SGEM
SGEM GeoConference

International Scientific GeoConference SGEM

Explore the main SGEM WORLD SCIENCE forum for Earth and Planetary Sciences, where research becomes conference presentation, proceedings publication and long-term library visibility.

Visit sgem.org
SGEM Vienna Green
SGEM Vienna Green

Green Sciences and Sustainability

Explore SGEM Vienna Green — connecting sustainability, environmental science, climate research, green technologies and interdisciplinary solutions for the future.

Visit sgemviennagreen.org

International Indexing & Global Visibility of Our Scientific Publications

SGEM scientific publications gain international visibility through a broad network of scholarly indexing and abstracting databases, citation-tracking services, research discovery platforms, and academic repositories.

Depending on the platform, our publications may be accessible as indexed bibliographic records, abstracts, citation data, DOI-linked metadata, or full-text scientific papers. Coverage and availability vary across platforms and publication years.

Scopus

Scopus Scientific Database

Compendex

Engineering abstracts
& indexing

Clarivate Databases

Scientific Databases

EBSCO

EBSCO
Science Services Database

OpenAIRE

Linked research discovery
& metadata

ProQuest

Scientific Databases
Part of Clarivate

Ulrichsweb

Global serials directory
Part of Clarivate

Crossref

We are a voting CrossRef member - the official DOI provider

Dimensions

Research discovery, citations
& metadata

ScienceOpen

Research discovery
& metadata

HAL

Multidisciplinary archive
& metadata

Petroleum Abstracts

Scientific Database
Part of Clarivate

Google Scholar

Google Scholar
Scholarly Search

Scilit

Scientific literature discovery
& metadata

RSCI

Russian Science Citation Index
Part of Web of Science

OpenAlex

Open research index
& metadata

Mendeley

Scientific Databases
Part of Elsevier

GeoRef

GeoRef — AGI
Geoscience Bibliographic Database